To make the life more colorful
To paste the PVC Wood Grain Decorative Film, you need to start with these methods. First, clean the contact surface of the film. The specific requirements are that there are no burrs, no oil traces, no splices, and if there are uneven places, you need to use atomic After filling the gaps, nail holes and incomplete positions, sand it with fine sandpaper until it is flat. Then use a special primer to spread the contact surface evenly, wait for it to dry, polish it again, remove the glue point on it, and then apply the film. When sticking the film, do not stick the whole surface at one time, you need to rush from one end to the other end, which can reduce the generation of air bubbles. When the wood grain film is applied, we have different operation methods for different contact surface base layers. The specific steps are as follows:
1. Construction method of plane base wood grain film
1. The contact surface needs to be ground and treated in combination with the above basic operating requirements.
2. Use a tape measure to measure the size of the area of the film, and then cut it out. Do not tear off the release paper. Test the position first to avoid cutting too large or too small, and then apply the film after confirming that it is suitable.
3. Remove the release paper about 5-10 cm from one side, and then stick it on one end first, and fix the bottom position to avoid tilting. Then press the film from top to bottom, remove 5-10 cm of release paper at a time, and slowly press and push the air out.
4. After pasting, use a scraper and a wallpaper knife to remove the excess corners, and the small air bubbles in the large surface can be punctured with a wallpaper knife and then flattened by exhausting air.
2. Right-angle film construction of wood grain film
1. Apply base oil to the base layer, the ratio can be diluted according to 1:1, and then wait for it to fully dry, and then polish it flat.
2. After sticking one side firmly, put on gloves at the corners to press out direct marks, do not pull them directly, this will cause a lot of bubbles to appear in the corners, and stick the right angles into rounded corners.
3. Then use a hot air blower to blow and compact it, so as to avoid the problem of separation and peeling in the later stage.
3. Construction method of concave right angle film
1. The base layer also needs to be ground, and the right angles are ground. Then apply a primer and smooth it out after application.
2. Press out the right angle on one side first, then do not compress the wood grain film at the right angle at the bottom, use a scraper to press out the right angle at the bottom, and then the middle position of the concave surface can be laminated by lamination. , and the excess part can be cut off.
There are many different contact surfaces that need to be constructed in the film of wood grain film. When filming, we should not ignore the details in order to save trouble, which will lead to the failure of PVC Wood Grain Decorative Film.